Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3ZG6 BK20591 - PA66-I-GF30 - BASF

Material Data Center offers the following functions for Ultramid® A3ZG6 BK20591:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
An impact-modified, glassfibre reinforced injection moulding grade with good dimensional stability.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 15 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.5 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.9 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 8500 / 6000 MPa ISO 527
Stress at break 140 / 100 MPa ISO 527
Strain at break 3.5 / 6 % ISO 527
Tensile creep modulus, 1000h * / 3000 MPa ISO 899-1
Charpy impact strength, +23°C 90 / 95 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 85 / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 19 / 26 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 10 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 260 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 240 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 250 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 27 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 128 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Yellow Card available yes / * - -
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 0.8 / * mm -
Yellow Card available yes / * - -
Burning rate, FMVSS, Thickness 1 mm 0 mm/min ISO 3795 (FMVSS 302)
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3.5 / 5.5 - IEC 62631-2-1
Dissipation factor, 1MHz 140 / 1600 E-4 IEC 62631-2-1
Volume resistivity 1E13 / 1E10 Ohm*m IEC 62631-3-1
Surface resistivity * / 1E10 Ohm IEC 62631-3-2
Comparative tracking index - / 550 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 5 / * % Sim. to ISO 62
Humidity absorption 1.5 / * % Sim. to ISO 62
Density 1330 / - kg/m³ ISO 1183
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 160 / * cm³/g ISO 307, 1157, 1628
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 290 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.15 % -
Melt temperature 280 - 300 °C -
Mold temperature 80 - 90 °C -
Diagrams
Viscosity-shear rate , Ultramid® A3ZG6 BK20591, PA66-I-GF30, BASF
Shearstress-shear rate , Ultramid® A3ZG6 BK20591, PA66-I-GF30, BASF
Dynamic Shear modulus-temperature , Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Dynamic Shear modulus-temperature , Ultramid® A3ZG6 BK20591 (cond.), PA66-I-GF30, BASF
Stress-strain , Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Stress-strain , Ultramid® A3ZG6 BK20591 (cond.), PA66-I-GF30, BASF
Secant modulus-strain , Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Secant modulus-strain , Ultramid® A3ZG6 BK20591 (cond.), PA66-I-GF30, BASF
Stress-strain (isochronous) 23°C, Ultramid® A3ZG6 BK20591 (cond.), PA66-I-GF30, BASF
Creep modulus-time 23°C, Ultramid® A3ZG6 BK20591 (cond.), PA66-I-GF30, BASF
Creep curve 23°C, Ultramid® A3ZG6 BK20591 (cond.), PA66-I-GF30, BASF
Stress-strain (isochronous) 80°C, Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Creep modulus-time 80°C, Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Creep curve 80°C, Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Stress-strain (isochronous) 120°C, Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Creep modulus-time 120°C, Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Creep curve 120°C, Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Tensile modulus-temperature , Ultramid® A3ZG6 BK20591 (dry), PA66-I-GF30, BASF
Tensile modulus-temperature , Ultramid® A3ZG6 BK20591 (cond.), PA66-I-GF30, BASF
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black
Additives
Lubricants, Release agent
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 300 °C
injection molding, Melt temperature, recommended: 290 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.